Title:
Creep properties and fracture mechanism of P92 steel used in ultra-supercritical power plant
文章编号:
1671-7627(2014)03-0032-07
作者:
王小威巩建鸣郭晓峰姜勇
南京工业大学 机械与动力工程学院,江苏 南京 211800
Author(s):
WANG XiaoweiGONG JianmingGUO XiaofengJIANG Yong
College of Mechanical and Power Engineering, Nanjing Tech University, Nanjing 211800, China
关键词:
超超临界发电 国产P92钢 蠕变 断裂 Larson-Miller
Keywords:
ultra-supercritical power plant domestic P92 steel creep fracture Larson-Miller
分类号:
TG142.15;TK226
DOI:
10.3969/j.issn.1671-7627.2014.03.007
文献标志码:
A
摘要:
P92钢因其在高温条件下具有优异的抗氧化性能、高温蠕变性能以及较低的热膨胀系数,而被广泛应用于超超临界发电厂的主蒸汽管道等厚壁部件。通过625、650 ℃不同应力条件下的高温蠕变试验以及运用金相显微镜(OM)、扫描电子显微镜(SEM)等微观分析技术对国产P92钢的蠕变特性及断裂机制进行了分析,并与国外生产的P92钢进行比较。结果表明:国产P92钢最小蠕变速率和蠕变破断寿命与蠕变应力之间的关系均遵循幂定律; 国产P92钢的蠕变寿命明显低于国外P92钢,蠕变过程中Laves相的迅速长大和粗化是国产P92钢蠕变性能劣化的主要原因; Larson-Miller方法中,参数C=38时拟合的Larson-Miller曲线可以很好地与试验值吻合。
Abstract:
ASME P92 steel was widely used in ultra-supercritical power plant due to its excellent oxidation resistance, good combination of creep strength in high temperature and low thermal expansion coefficient. Creep experiments were conducted under different stress conditions at 625 ℃ and 650 ℃. Then, the creep characteristics and the fracture mechanism of domestic P92 steel were analyzed by a micro-analytic technique, such as optical microscope(OM)and scanning electron microscope(SEM). Finally, results were compared between domestic and foreign P92 steels. The stress dependence of minimum creep rate and creep rupture life of domestic P92 obeyed power law. The creep life of domestic P92 steel was obviously lower than that of foreign steel, the fast growth and coarsening of Laves phase were the main reasons for domestic P92 steel premature creep rupture. Experimental data were fitted with Larson-Miller curves when C=38.

参考文献/References:

[1] Bugge J,Kjaer S,Blum R.High-efficiency coal-fired power plants development and perspectives [J].Energy,2006,31(10):1437-1445.
[2] Brozda J.New generation creep-resistant steels,their weldability and properties of welded joints:T/P92 steel[J].Welding International,2005,19(1):5-13.
[3] 潘志强,胡恒康,曾凤鸣,等.百万级火电机组主蒸汽管道缺陷检测探讨[J].中国电机工程学报,2009,29:135-137.
[4] Pesicka J,Kuzel R,Dronhofer A,et al.The evolution of dislocation density during heat treatment and creep of tempered martensite
   ferritic steels[J].Acta Materialia,2003,51(46):4847- 4862.
[5] Yoshizawa M,Igarashi M,Moriguchi K,et al.Effect of precipitates on long-term creep deformation properties of P92 and P122 type advanced ferritic steels for USC power plants[J].Materials Science and Engineering:A,2009,510:162-168.
[6] Lee J S,Armaki H G,Maruyama K,et al.Causes of breakdown of creep strength in 9Cr-1.8W-0.5Mo-VNb steel[J].Materials Science and Engineering:A,2006,428(1):270-275.
[7] Abe F.Analysis of creep rates of tempered martensitic 9%Cr steel based on microstructure evolution[J].Materials Science and Engineering:A,2009,510:64-69.
[8] Sawada K,Kubo K,Abe F.Creep behavior and stability of MX precipitates at high temperature in 9Cr-0.5Mo-1.8W-VNb steel[J].Materials Science and Engineering:A,2001,319:784-787.
[9] 张红军,周荣灿,唐丽英,等.P92钢650 ℃时效的组织性能研究[J].中国电机工程学报,2009,29:174-177.
[10] Hald J.Microstructure and long-term creep properties of 9%-12% Cr steels[J].International Journal of Pressure Vessels and Piping,2008,85(1):30-37.
[11] Vailiant J C,Vandenberghe B,Hahn B,et al.T/P23,24,911 and 92:new grades for advanced coal-fired power plants-properties and experience[J].Pressure Vessels and Piping,2008,85(1):38- 46.
[12] Park K S,Masuyama F,Endo T.Creep modeling for life evaluation of heat-resistant steel with a martensitic structure[J].ISIJ International,2001,41:S86-S90.
[13] Petry C,Lindet G.Modelling creep behaviour and failure of 9Cr-0.5Mo-1.8W-VNb steel[J].International Journal of Pressure Vessels and Piping,2009,86(8):486-494.
[14] 任纬丽,郭建亭,周继扬.两相共晶NiAl-9Mo合金的蠕变行为[J].金属学报,2002,38(9):908-913.
[15] Sklenicka V,Kucharova K,Svoboda M,et al.Long-term creep behavior of 9%-12%Cr power plant steels[J].Materials Characterization,2003,51(1):35-48.
[16] Masuyama F.Creep rupture life and design factors for high-strength ferritic steels[J].International Journal of Pressure Vessels And Piping,2007,84(1):53-61.
[17] 戴长清,田富强,轩福贞.锅炉管道用9%-12%Cr钢Larson-Miller公式C参数确定[J].化工设备与管道,2010,47(1):55-58.
[18] Kimura K,Sawada K,Kubo K,et al.Influence of stress on degradation and life prediction of high strength ferritic steels[C]//ASME 2004 pressure vessels and Piping Conference.[s.l.]:American Society of Mechanical Engineers,2004:11-18.